A Precise and Scalable Post-Modification of Mesoporous Metal-Organic Framework NU-1000 Via Atomic Layer Deposition

Metal Organic Frameworks

Publication Details

  • Authors: I.S. Kim, O.K. Farha, J. T. Hupp, L. Gagliardi, K. W. Chapman, C. Cramer, and A. B. F. Martinson
  • Publication Number: 247
  • Year: 2016
  • Journal: ECS Trans.

Full Citation

I.S. Kim, O.K. Farha, J. T. Hupp, L. Gagliardi, K. W. Chapman, C. Cramer, and A. B. F. Martinson, A Precise and Scalable Post-Modification of Mesoporous Metal-Organic Framework NU-1000 Via Atomic Layer Deposition, ECS Trans., 2016, 75, 93–99. DOI: 10.1149/07506.0093ecst